A casting defect formed, when two stream of liquid metal meet without complete fusion is known as:
CUET (PG) - 2023
CUET (PG)
Updated On:
Mar 21, 2024
Cold shut
Mismatch
Flash
Scab
Hide Solution
Verified By Collegedunia
The Correct Option is
A
Solution and Explanation
The correct option is (A): Cold shut
Download Solution in PDF
Was this answer helpful?
0
0
Questions Asked in CUET PG exam
Upper palaeolithic culture in India is dominated by:
CUET (PG) - 2025
Prehistoric Archaeology
View Solution
Which of the following species are included among gracile australopithecines?
A. A. africanus
B. A. boisei
C. A. afarensis
D. A. anamensis
Choose the correct answer from the options given below:
CUET (PG) - 2025
Paleoanthropology
View Solution
A bought an article at a certain price and sold it at 10% profit. B bought the same article at a price 10% lesser than A and sold it at ₹18 lesser than A. B's gain percentage in this deal is 20%. At what price B bought the article?
CUET (PG) - 2025
Profit and Loss
View Solution
The traffic lights at three different road crossings change after every 48 seconds, 72 seconds and 108 seconds respectively. If they all change simultaneously at 8:20:00 hours, then at what time will they again change simultaneously?
CUET (PG) - 2025
Quantitative Aptitude
View Solution
In terracotta which materials are mainly used to build strong clay
(A) Grog
(B) Metal
(C) Cotton
(D) Stone
Choose the correct answer from the options given below:
CUET (PG) - 2025
Ceramics and Pottery
View Solution
View More Questions