Step 1: The form of iron obtained from the blast furnace is pig iron, which is then further refined to produce cast iron. Step 2: Pig iron contains high amounts of carbon (3-4%) and impurities, while cast iron is obtained by refining pig iron and lowering its carbon content. Step 3: Wrought iron is produced by further refining cast iron, removing most of the carbon and impurities.